Structural Specifications
for Tridipanel System
PART
5 - PERFORMANCE CHARACTERISTICS
5 - 1 SIZES:
A. Panels
are 4 feet wide and can be produced in lengths from 8 feet to 25 feet
in increments of 8". Panel thickness ranges from 3 1/4" to 5
1/4" depending on thickness of polystyrene specified.
B. Dimensional
tolerance - the tolerances shall comply with values listed in the manufacturers
quality assurance procedures.
Note: Overall
length ± 1/4" - 12' L or less, ± 1/2" - 12' L or
more.
Overall width ± 1/8"
Overall thickness ± 1/4"
Location of truss wires within units ± 1/2"

|

Pre-Installing
Windows Before Shotcreting
|
5
- 2 STRUCTURAL TESTING:
Testing values of each panel shall meet or exceed
those loads on Manufacturer's Load Design Charts. These charts were developed
from results of tests conducted in accordance with ASTM E-72 and with
provisions of ACI-318.
5
- 3 FIRE RESISTANCE:
Based on fire resistance calculations and the results
of the Modified E - 108 Fire Test performed at Southwest Research Institute
(SW RI Project No. 01-2601-407) the following fire resistance ratings
may be assigned to the 3-D panels provided carbonate shotcrete is applied:
PART
6 - INSTALLATION
6 -1 Erection:
A. Prior
to erection the contractor or his representative shall inspect the site
and report to the construction manager any condition that may affect
the proper installation of the panels. Installation should not proceed
until these conditions are corrected.
B. 3 - D
Panel installation shall be carried out in strict accordance with the
latest edition of the Manufacture's Instructions for 3 - D Panel System
Erection. For any field deviation from standard load design, values
shall be calculated and approved and signed or sealed by a qualified
architect/engineer.
|

Binding and
Fitting Support Corners
|
6 - 2 Concreting
Practice:
Concrete
can be applied by several methods; however, all concrete shall meet a
minimum of 2,500 psi. All shotcrete construction, including materials,
equipment, preliminary preparation, proportioning, shotcrete placement,
curing and quality control shall comply with ACI 506R-85 Guide to shotcrete.
6 - 3 Testing:
A. An important
aspect of quality control is the physical testing of the concrete during
and after placement. ACI 506.2 describes in full the procedures to be
followed in construction testing.
B. Normal
testing ages for compressive strength are 7 and 28 days; however, shorter
periods may be required under particular application or conditions.
Telephone (760) 643-2307, Fax (760) 643-2305 or E-Mail
us.